Bioprocessing (English only)
Accelerate your biologic
drug development with
Purolite™ chromatography resins.
Accelerate your biologic
drug development with
Purolite™ chromatography resins.
私たちは樹脂技術のグローバルリーダーとして、世界で最も規制の厳しい産業で、非常に特殊な元素や化合物を分離、除去、回収するために使用される小型ビーズを開発・製造しています。
もっと読むWith 40 years of manufacturing expertise and 30 years of regulatory experience, we supply leading separation, purification and extraction technologies to support chromatography applications within the Pharma and Medical space.
Learn moreWe are a world leader in resin-based separation, purification and extraction technology, that provides sustainable solutions for our environment, businesses and healthcare.
Learn More* SST®はピュロライト社の登録商標
Polymer Structure | ジビニルベンゼンにより架橋されたポリスチレンゲル | |
Appearance | 球形ビード | |
Functional Group | 硫酸 | |
Ionic Form | Na+形 | |
乾燥樹脂当たり交換容量 (最小) | 3.8 当量 / kg (Na+形) | |
水分含有率 | 38 - 46 % (Na+形) | |
粒径範囲 | 300 - 1200 µm | |
< 300 µm (max.) | 1 % | |
均一係数 (最大) | 1.7 | |
可逆的膨張, Na+ → H+(最大) | 8 % | |
比重 | 1.2 | |
見かけ密度 (概算) | 775 - 825 g/L (48.4 - 51.6 lb/ft³) | |
温度制限 | 60 °C (140.0 °F) |
The pressure drop across a bed of ion exchange resin depends on the particle size distribution, bed depth, and voids volume of the exchange material, as well as on the flow rate and viscosity of the influent solution. Factors affecting any of these parameters— such as the presence of particulate matter filtered out by the bed, abnormal compressibility of the resin, or the incomplete classification of the bed—will have an adverse effect, and result in an increased head loss. Depending on the quality of the influent water, the application and the design of the plant, service flow rates may vary from 10 to 40 BV/h.
During up-flow backwash, the resin bed should be expanded in volume between 50 and 70% for at least 10 to 15 minutes. This operation will free particulate matter, clear the bed of bubbles and voids, and reclassify the resin particles ensuring minimum resistance to flow. When first putting into service, approximately 30 minutes of expansion is usually sufficient to properly classify the bed. It is important to note that bed expansion increases with flow rate and decreases with influent fluid temperature. Caution must be taken to avoid loss of resin through the top of the vessel by over expansion of the bed.