Overview
Literature

Principal Applications

  • 6価クロムイオン除去
  • ウラン- 除去
  • 硫酸除去

Advantages

  • 高交換容量
  • 非常に高い物理的安定性
  • 高い反応速度

Regulatory Approvals

  • Compliant with FDA Regulation 21 CFR 173.25 for Food Treatment, Ion Exchangers
  • 水の規制に関する諮問制度認可
  • WQAによるNSF/ANSI-61 Standard証明書
  • コーシャ認定
  • IFANCA Halal認定

Typical Packaging

  • 1 ft³ Sack
  • 25 L Sack
  • 5 ft³ Drum (Fiber)
  • 1 m³ Supersack
  • 42 ft³ Supersack

* PGW6002EはA600E/9149より25%高い運転交換容量を持ちます

Typical Physical & Chemical Characteristics:

Polymer Structure ジビニルベンゼンにより架橋されたポリスチレンゲル
Appearance 球形ビード
Functional Group Ⅰ型4級アンモニウム
Ionic Form Cl-
総交換容量(最小) 1.65 eq/l (36.1 Kgr/ft³) (Cl-)
水分含有率 40 - 45 % (Cl-)
平均径 570 ± 50 µm
< 425 µm (max.) 1 %
均一係数 (最大) 1.2
比重 1.09
見かけ密度 (概算) 675 - 710 g/L (42.2 - 44.4 lb/ft³)
温度制限 100 °C (212.0 °F) (Cl-)
温度制限 60 °C (140.0 °F) (OH- 形)

油圧特性

Pressure Drop

The pressure drop across a bed of ion exchange resin depends on the particle size distribution, bed depth, and voids volume of the exchange material, as well as on the flow rate and viscosity of the influent solution. Factors affecting any of these parameters— such as the presence of particulate matter filtered out by the bed, abnormal compressibility of the resin, or the incomplete classification of the bed—will have an adverse effect, and result in an increased head loss. Depending on the quality of the influent water, the application and the design of the plant, service flow rates may vary from 10 to 40 BV/h.

Pressure Drop Across Resin Bed

Backwash

A 20 BV downflow rinse is required before the vessel is put into service. This rinse can be done onsite or offsite pre-installation. Once the resin is put into service, backwashing is not permitted as this will lead to shortened bed life. This is a uniform grade resin with beads of similar size and will not require backwashing for classification / stratification before use. If it is determined, before startup, that air bubbles or particulate matter are trapped within the bed, then backwashing can be done. In that case, the resin bed should be expanded by 50-70% for 10-15 minutes. Please note that bed expansion increases with higher flow rate and lower water temperature. Avoid loss of resin through the top of the vessel by over expansion of the bed.