Overview
Literature

主要应用

  • Removal of perfluoroalkyl substances
  • Removal of polyfluoroalkyl substances

产品优势

  • 非常高的工作交换容量
  • 优良的动力学性能
  • 将全氟辛烷磺酸降低到万亿分之一到万亿分之五的非检测水平

包装样式

  • 1 CF 编织袋
  • 25L 阀口袋
  • 5 CF 纤维板桶
  • 1M3 立方袋
  • 42 ft³ 立方袋

典型物理和化学参数

聚合物骨架 聚苯乙烯二乙烯苯交联
外观 球状颗粒
官能团 复合氨
粒径分布 425 - 1180 µm
< 425 µm (最大) 2 %
均一系数(最大) 1.6
比重 1.05
包装密度(大约) 650 - 700 g/L (40.6 - 43.8 lb/ft³)
温度限制 100 °C (212.0 °F) (Cl-型)
温度限制 60 °C (140.0 °F) (OH- 型)

水力学特性

Pressure Drop

The pressure drop across a bed of ion exchange resin depends on the particle size distribution, bed depth, and voids volume of the exchange material, as well as on the flow rate and viscosity of the influent solution. Factors affecting any of these parameters— such as the presence of particulate matter filtered out by the bed, abnormal compressibility of the resin, or the incomplete classification of the bed—will have an adverse effect, and result in an increased head loss. Depending on the quality of the influent water, the application and the design of the plant, service flow rates may vary from 10 to 40 BV/h.

Pressure Drop Across Resin Bed

反洗

在自下而上反洗过程中,应控制反洗膨胀率在50%到70%之间,至少保持10到15分钟。 该操作除去(运行过程中截留的物料中的)颗粒物,清除气泡,并重新规整树脂颗粒,确保最小的流动阻力。 第一次投入前,大约30分钟的充分反洗,通常就足以对树脂床层进行适当的规整。 值得注意的是,相同流速下反洗膨胀率随温度降低而而升高。 必须注意,应避免将树脂床层反洗膨胀过甚而导致树脂从顶部流失。

树脂床反洗膨胀率