Overview

Principal Applications

  • Demineralization - High Purity Water

Advantages

  • High operating capacity
  • Excellent resistance to osmotic shock
  • Uniform particle size
  • Antistat treated for easier separation from cation component

Systems

  • Condensate polishing mixed beds
  • Makeup Polishing Mixed Bed
  • RO Polishing Mixed Bed
  • Working Mixed Bed

Typical Packaging

  • 1 ft³ Sack
  • 25 L Sack
  • 5 ft³ Drum (Fiber)
  • 1 m³ Supersack
  • 42 ft³ Supersack

Typical Physical & Chemical Characteristics:

Polymer Structure Gel polystyrene crosslinked with divinylbenzene
Appearance Spherical Beads
Functional Group Type I Quaternary Ammonium
Ionic Form OH-
Total Capacity (min.) 1.1 eq/L (24.0 Kgr/ft³) (OH- form)
Moisture Retention 54 - 63 % (OH- form)
Mean Diameter 590 ± 50 µm
Uniformity Coefficient (max.) 1.2
< 300 µm (max.) 0.5 %
< 850 µm (min.) 99 %
Whole Beads (min.) 99 %
Conversion (min.) 90 % (OH- form)
Average Breaking Weight (min.) 350 g
Breaking Weight <200 g (max.) 5 %
Reversible Swelling, Cl- → OH- (max.) 24 %
Specific Gravity 1.08
Shipping Weight (approx.) 660 - 700 g/L (41.2 - 43.8 lb/ft³)
Residual Iron (max.) 100 ppm
Residual lead (max.) 50 ppm
Residual Aluminum (max.) 50 ppm
Residual Copper (max.) 50 ppm
Temperature Limit 100 °C (212.0 °F) (Cl- form)
Temperature Limit 60 °C (140.0 °F) (OH- form)
Recommended Mixed Bed Pairing Purolite™ Select SRC6500H, SRC6500Na

Hydraulic Characteristics

Pressure Drop

The pressure drop across a bed of ion exchange resin depends on the particle size distribution, bed depth, and voids volume of the exchange material, as well as on the flow rate and viscosity of the influent solution. Factors affecting any of these parameters— such as the presence of particulate matter filtered out by the bed, abnormal compressibility of the resin, or the incomplete classification of the bed—will have an adverse effect, and result in an increased head loss. Depending on the quality of the influent water, the application and the design of the plant, service flow rates may vary from 10 to 40 BV/h.

Pressure Drop Across Resin Bed