New Product
DurA Cycle A50
Driving innovation and performance while
reducing cost of goods.
DurA Cycle A50
Driving innovation and performance while
reducing cost of goods.
As a global leader in resin technology, we develop and manufacture small beads that are used in the most regulated industries in the world to separate, remove or recover very specific elements and compounds.
Learn MoreWith 40 years of manufacturing expertise and 30 years of regulatory experience, we supply leading separation, purification and extraction technologies to support chromatography applications within the Pharma and Medical space.
Learn moreWe are a world leader in resin-based separation, purification and extraction technology, that provides sustainable solutions for our environment, businesses and healthcare.
Learn MorePolyacryl makroporös, Chlorid Form
Unsere stets einsatzbereiten technischen Support- und Serviceteams gehen noch einen Schritt weiter, um Ihre vertrauenswürdigste Ressource zu sein. Wir sind für Sie da.
Polymerstruktur | makroporöses polyacryl quervernetzt mit Divinylbenzol | |
Aussehen | Spherische Kugeln | |
Funktionelle Gruppe | quartäres Ammonium | |
Ionische Form | Cl- | |
Totalkapazität (min.) | 0.8 eq/L (17.5 Kgr/ft³) (Cl-) | |
Wassergehalt | 66 - 72 % (Cl-) | |
Partikelgrößen Bereich | 300 - 1200 µm | |
Uniformitätskoeffizient (max) | 1.7 | |
Volume Change Cl- → OH- (max.) | 30 % | |
Spezifische Dichte | 1.08 | |
Schüttgewicht (ca.) | 680 - 730 g/l (42.5 - 45.6 lb/ft³) | |
Temperaturlimit | 80 °C (176.0 °F) (Cl-) |
During up-flow backwash, the resin bed should be expanded in volume between 50 and 70% for at least 10 to 15 minutes. This operation will free particulate matter, clear the bed of bubbles and voids, and reclassify the resin particles ensuring minimum resistance to flow. When first putting into service, approximately 30 minutes of expansion is usually sufficient to properly classify the bed. It is important to note that bed expansion increases with flow rate and decreases with influent fluid temperature. Caution must be taken to avoid loss of resin through the top of the vessel by over expansion of the bed.